Mainly used for joint coating, damage repair of steel pipelines in petroleum, natural gas, chemical industry, urban gas pipeline networks, etc., as well as joint sealing and fixing of PE and PVC pipelines in engineering projects such as externally wrapped anti-corrosion and thermal insulation pipelines (clamped pipes) for joints, elbows, tees, and water supply and drainage.
Features
High mechanical strength, strong anti-aging ability, good sealing performance, corrosion resistance, convenient and fast construction, time and labor saving.
Notes
Materials can be customized according to different temperatures and regions.
Technical Data
Property
Test Method
TS50(mastic) (Typical value)
TS60 (Typical value)
Solids Content (%)
GB/T1728
99.5
99.5
Cathodic Disbondment (65℃, 48h) mm
Q/SYGJX0113-2007
8
8
Tensile Strength Mpa
GB/T1040-92
18
19
Elongation at Break %
GB/T1040-92
500
550
Dielectric Strength MV/m
GB/T1408.1-99
28
28
Volume Resistivity Ω·m
GB/T1410-89
4.0×1015
4.0×1015
Water Absorption %
ASTM D570-2005
0.02
0.02
Heat Aging (150℃, 21 days)
GB/T1040-92
Tensile Strength Mpa
17.0
18.0
Elongation at Break %
450
480
UV Aging Resistance
EN12068
Elongation at Break %
480
Softening Point ℃
GB/T4507-85
78
114
Peel Strength
To Primed Steel N/cm
To PE N/cm
GB/T2792-98
70
70
160
80
Cathodic Disbondment (70℃, 30d) mm
SY/T0413-2002
/
/
Hot Water Immersion
ASTM D870-2002
No delamination,
no water corrosion under test conditions
No delamination,
no water corrosion under test conditions
|
Size |
Applicable Pipe Diameter (mm) |
Heat Shrink Tubing Length (mm) |
Heat Shrinkage Rate (%) |
|
20-330-1.0 |
DN20 |
330 |
≥50 |
|
25-330-1.0 |
DN25 |
330 |
≥50 |
|
32-330-1.0 |
DN32 |
330 |
≥45 |
|
40-330-1.0 |
DN40 |
330 |
≥45 |
|
50-330-1.0 |
DN50 |
330 |
≥45 |
|
65-330-1.0 |
DN65 |
330 |
≥45 |
|
80-330-1.0 |
DN80 |
330 |
≥45 |